    I would also recommend Devilbiss digital gauge.

    February 24, 2013 at 8:33 pm #41616

    I would recommend also to check pressure, and, in general, to use only HVLP technology for base coats.

    February 24, 2013 at 8:27 pm #41615

    What is interesting, in Europe the tendency is in moving to one product instead of using filler and putty. The idea is to have one product for both filling and glazing. Our sales of fine putty are very small into comparison to universal polyester filler, which is rather normal specific wait, than light one.